The electroluminescence test is an experiment typically used to verify the behavior of the photovoltaic cell and to qualitatively check its integrity. It works by operating the photovoltaic cell as a diode polarized directly: the cells that light up in a module indicate how many of them work. This test provides an estimate of the maximum performance of the entire photovoltaic module. A qualitative inspection was performed by electroluminescence tests on 48 modules of photovoltaic cells. They had already been installed on a small-size concentration solar plant before the test and some modules had reached a lower level of performance than expected. A first electroluminescence test was performed, which showed that only 61.5% of the photocells worked. Since there were visible signs of humidity within the various modules, some of the inoperative modules underwent a dehumidification treatment in a climatic chamber. A second electroluminescence test showed that the percentage of functioning cells had increased to 66.3% after the drying treatment.
Electroluminescence test to investigate the humidity effect on solar cells operation / Fontani, Daniela; Sansoni, Paola*; Francini, Franco; Messeri, Matteo; Pierucci, Giacomo; DeLucia, Maurizio; Jafrancesco, David. - In: ENERGIES. - ISSN 1996-1073. - ELETTRONICO. - 11:(2018), pp. 2659-2674. [10.3390/en11102659]
Electroluminescence test to investigate the humidity effect on solar cells operation
Messeri, Matteo;Pierucci, Giacomo;DeLucia, Maurizio;
2018
Abstract
The electroluminescence test is an experiment typically used to verify the behavior of the photovoltaic cell and to qualitatively check its integrity. It works by operating the photovoltaic cell as a diode polarized directly: the cells that light up in a module indicate how many of them work. This test provides an estimate of the maximum performance of the entire photovoltaic module. A qualitative inspection was performed by electroluminescence tests on 48 modules of photovoltaic cells. They had already been installed on a small-size concentration solar plant before the test and some modules had reached a lower level of performance than expected. A first electroluminescence test was performed, which showed that only 61.5% of the photocells worked. Since there were visible signs of humidity within the various modules, some of the inoperative modules underwent a dehumidification treatment in a climatic chamber. A second electroluminescence test showed that the percentage of functioning cells had increased to 66.3% after the drying treatment.File | Dimensione | Formato | |
---|---|---|---|
energies-11-02659-v2.pdf
accesso aperto
Descrizione: articolo completo
Tipologia:
Pdf editoriale (Version of record)
Licenza:
Open Access
Dimensione
6.24 MB
Formato
Adobe PDF
|
6.24 MB | Adobe PDF |
I documenti in FLORE sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.