Abstract PURPOSE: To compare the bond strength to human primary dentin of a self-adhesive light-curing resin composite, a self-etch adhesive and a glass-ionomer cement by means of microshear bond strength (pSBS) test and scanning electron microscopic (SEM) observations. METHODS: 75 human primary molars were sectioned to obtain a 2 mm-thick slab of mid-coronal dentin, randomly divided into three groups (n=25). Nine conical frustum-shaped buildups were constructed on the occlusal surface of each dentin slab using a self-adhesive light-curing resin composite (Vertise Flow; Group 1), bonding agent (Optibond All-in-One; Group 2) combined with resin composite (Premise Flow) and a glass-ionomer cement (Ketac-Fil; Group 3). After thermocycling, specimens were subjected to microSBS test. All debonded specimens were observed at SEM. Data were analyzed by a mixed model and chi-square test. RESULTS: The bond strength measured in Group 1 (9.0 +/- 4.5 MPa) was significantly lower than that one recorded in Group 2 (20.2 +/-12.5 MPa) although it was significantly higher than the one recorded in Group 3 (4.8 +/- 2.3 MPa). Failures were mainly adhesive in all groups.

Adhesion to primary dentin: microshear bond strength and scanning electron microscopic observation / Scaminaci Russo D;Iuliano V;Franchi L;Ferrari M;Giachetti L. - In: AMERICAN JOURNAL OF DENTISTRY. - ISSN 0894-8275. - STAMPA. - 26:(2013), pp. 341-346.

Adhesion to primary dentin: microshear bond strength and scanning electron microscopic observation.

SCAMINACI RUSSO, DANIELE;FRANCHI, LORENZO;GIACHETTI, LUCA
2013

Abstract

Abstract PURPOSE: To compare the bond strength to human primary dentin of a self-adhesive light-curing resin composite, a self-etch adhesive and a glass-ionomer cement by means of microshear bond strength (pSBS) test and scanning electron microscopic (SEM) observations. METHODS: 75 human primary molars were sectioned to obtain a 2 mm-thick slab of mid-coronal dentin, randomly divided into three groups (n=25). Nine conical frustum-shaped buildups were constructed on the occlusal surface of each dentin slab using a self-adhesive light-curing resin composite (Vertise Flow; Group 1), bonding agent (Optibond All-in-One; Group 2) combined with resin composite (Premise Flow) and a glass-ionomer cement (Ketac-Fil; Group 3). After thermocycling, specimens were subjected to microSBS test. All debonded specimens were observed at SEM. Data were analyzed by a mixed model and chi-square test. RESULTS: The bond strength measured in Group 1 (9.0 +/- 4.5 MPa) was significantly lower than that one recorded in Group 2 (20.2 +/-12.5 MPa) although it was significantly higher than the one recorded in Group 3 (4.8 +/- 2.3 MPa). Failures were mainly adhesive in all groups.
2013
26
341
346
Scaminaci Russo D;Iuliano V;Franchi L;Ferrari M;Giachetti L
File in questo prodotto:
File Dimensione Formato  
Scaminaci Russo AJD Dec 2013.pdf

Accesso chiuso

Tipologia: Versione finale referata (Postprint, Accepted manuscript)
Licenza: Tutti i diritti riservati
Dimensione 258.31 kB
Formato Adobe PDF
258.31 kB Adobe PDF   Richiedi una copia

I documenti in FLORE sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificatore per citare o creare un link a questa risorsa: https://hdl.handle.net/2158/849909
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 8
  • ???jsp.display-item.citation.isi??? 7
social impact